AMA · AF-04 · FAA-H-8083-31B CH. 4
FAA A&P Airframe: Aircraft Metal Structural Repair
For the FAA A&P Airframe test, aircraft sheet metal structural repair is chapter 4 of FAA-H-8083-31B, Aircraft Metal Structural Repair. Its ACS subject area, Metallic Structures, is 5 to 15% of the test, or 5 to 15 of its 100 scored questions. Our question bank holds 445 questions on it, and the 10 below were written for this page.
Test shares and most-missed codes read from the FAA on 15 November 2026.
What FAA-H-8083-31B chapter 4 covers
Chapter 4 is the biggest chapter in the Airframe handbook. It covers the stresses in structural members, the aluminum alloys and their tempers, the tools for layout, cutting, hole making and forming, and forming sheet metal: bend allowance, setback, the flat pattern and relief holes.
Then riveting: identifying solid rivets, laying out rivets with the right edge distance and pitch, installing, inspecting and removing them, and the special fasteners such as blind rivets. The last part covers inspecting and classifying damage and repairing skins, stringers, formers, ribs and spars, pressurized structure included.
It runs from pages 4-1 to 4-114 of the Aviation Maintenance Technician Handbook: Airframe, which the FAA publishes free as a PDF.
How much of the FAA A&P Airframe test it is
- 5 to 15%OF THE TESTACS area AM.II.A
- 5 to 15QUESTIONSof 100 scored
- 445IN OUR BANKquestions on this subject
The FAA’s Companion Guide to the ACS gives every subject area a range, not a count. Metallic Structures (AM.II.A) is 5 to 15% (5 to 15 questions) on the 100-question Airframe test. The 15 ranges for the Airframe test add up to anywhere from 75% to 160%, so they say how big an area can get, not how many questions you will see from it.
Metallic Structures is not ours alone to cover: our Aircraft Structures, Aircraft Welding and Aircraft Painting and Finishing questions are written to the same area.
No code in this area is on the FAA’s latest list of most-missed codes (2nd Quarter, CY25), which names a code only when it was missed more than 70% of the time on at least 100 tests.
Aircraft sheet metal structural repair questions and answers
10 questions in the test’s own format, each with 3 options and 1 correct answer. Pick yours, then open it to see the answer and the reason. Each one names the page it was written from, so you can check it.
- Q.01
The repair data for a wing skin repair does not give a rivet size. Where on the airplane can you look to see what size the manufacturer would have used?
FAA-H-8083-31B, ch. 4, p. 4-32
- AThe next parallel row outboard on the wing, toward the tip
- BThe next parallel row inboard on the wing, toward the root
- CThe screws in the nearest access panel, which match the skin
SHOW THE ANSWERHIDE THE ANSWER
THE ANSWER IS B.
The next parallel row inboard on the wing, toward the root
The right size of rivet for a repair can be found from the rivets the manufacturer used in the next parallel row inboard on the wing, or forward on the fuselage. Wing loads build toward the root, so an inboard row is sized for at least the load the repair area sees, while a row toward the tip may be sized for less. Access panels are held with screws, which tell you nothing about the rivet pattern the skin needs.
- Q.02
You are about to use a new set of joggling dies for the first time, on parts you have already made. What should you do first?
FAA-H-8083-31B, ch. 4, p. 4-81
- AHeat the dies so the metal flows into the joggle more easily
- BGrease the parts heavily so the dies cannot mark them
- CTry the dies on a piece of waste stock to check their accuracy
SHOW THE ANSWERHIDE THE ANSWER
THE ANSWER IS C.
Try the dies on a piece of waste stock to check their accuracy
Joggling dies used for the first time are tested for accuracy on a piece of waste stock, so a die that is off does not ruin parts that have already been made. The surfaces of the blocks are kept free of dirt and filings so the work is not marred. Neither heating the dies nor greasing the parts is part of the procedure.
- Q.03
One rivet in a skin joint is found loose. Why does it not necessarily overload the rivets next to it to the point of cracking?
FAA-H-8083-31B, ch. 4, p. 4-92
- ARivet patterns are normally sized as if one or more rivets carry no load
- BThe skin around a loose rivet stiffens and picks up its share of load
- CA loose rivet still carries its full shear load through its shank
SHOW THE ANSWERHIDE THE ANSWER
THE ANSWER IS A.
Rivet patterns are normally sized as if one or more rivets carry no load
It is common practice to size a rivet pattern on the assumption that one or more of its rivets is not doing its job. So a single loose rivet would not necessarily overload its neighbors to the point of cracking, and airframe cracking is not necessarily caused by defective rivets. A loose rivet does not carry its full share of load, and the skin does not stiffen to make up for it.
- Q.04
A flange on an aluminum part already has its rivet holes drilled, and now it has to be stretched to fit a curve. What does forming it with those holes in place risk?
FAA-H-8083-31B, ch. 4, p. 4-26
- AThe flange loses its temper and has to be heat treated again
- BThe holes distort and may crack, which can badly weaken the flange
- CNothing, since the holes act as relief holes that stop any cracking
SHOW THE ANSWERHIDE THE ANSWER
THE ANSWER IS B.
The holes distort and may crack, which can badly weaken the flange
Stretching thins the metal between the dies as they shift outward, and even a moderately stretched flange edge is best deburred or polished first so cracks do not start there. Forming a flange that already has holes in it makes those holes distort and possibly crack, which can substantially weaken the flange. Taking the temper out of metal is what annealing does, not stretching, and relief holes are placed where the inside bend tangent lines of 2 bends meet, not in a flange about to be stretched.
- Q.05
On a part that carries bending loads, the factory rivets are spaced close to the minimum pitch. When you repair it, why keep that close spacing?
FAA-H-8083-31B, ch. 4, p. 4-34
- AIt keeps the skin from buckling between the rivets
- BIt leaves room to drill the holes oversize later
- CIt lets the joint hold air without any sealant
SHOW THE ANSWERHIDE THE ANSWER
THE ANSWER IS A.
It keeps the skin from buckling between the rivets
Rivet pitch can be as small as 3 rivet diameters, usually runs 4 to 6, and can go as wide as 10. On parts subjected to bending moments the spacing is often held close to the minimum, because skin left unsupported over a longer span between rivets can buckle. It is spacing at least 1/16 inch over the minimum that leaves room to oversize a hole later, and a riveted joint is not airtight without seals or coatings.
- Q.06
You are bending a flange over a forming block with a mallet, and a large part of the sheet sticks out beyond the blocks. What should you do with the part that sticks out?
FAA-H-8083-31B, ch. 4, p. 4-74
- AClamp a heavy weight to its free end so it bends evenly
- BLet it hang free so your hands cannot mark it
- CKeep hand pressure on it so it does not bounce
SHOW THE ANSWERHIDE THE ANSWER
THE ANSWER IS C.
Keep hand pressure on it so it does not bounce
The protruding metal is worked down against the forming block a little at a time, and driven slightly past the angle wanted to allow for springback. When a large amount of metal sticks out beyond the blocks, hand pressure is kept on the protruding sheet to stop it bouncing as it is struck. Letting it hang free lets it bounce, and a weight clamped to the end is not part of the method.
- Q.07
You are repairing a sheet-metal seaplane float with approved practices. How should the seams between its sheet metal sections be treated?
FAA-H-8083-31B, ch. 4, p. 4-97
- AWaterproofed with suitable fabric and sealing compound
- BLeft dry, since the rivets seal a float's seams on their own
- CWelded along their full length so that no sealant is needed
SHOW THE ANSWERHIDE THE ANSWER
THE ANSWER IS A.
Waterproofed with suitable fabric and sealing compound
Sheet-metal floats are repaired with approved practices, and the seams between the sections of sheet metal are waterproofed with suitable fabric and sealing compound. Rivets alone do not make a seam watertight, which a float must be, and welding the seams is not the method the handbook gives for a riveted float.
- Q.08
After driving a rivet, you see the sheet around it has bulged toward the shop head. What is the most likely cause?
FAA-H-8083-31B, ch. 4, p. 4-35
- AThe bucking bar was too heavy for the job
- BThe rivet gun was set to too low a pressure
- CThe bucking bar was too light for the job
SHOW THE ANSWERHIDE THE ANSWER
THE ANSWER IS C.
The bucking bar was too light for the job
A bar that is too light does not give enough bucking weight, so the blows push the sheet out toward the shop head. A bar that is too heavy does the opposite and can bulge the material away from the shop head. Choosing a bar of the right shape and weight for the rivet avoids both.
- Q.09
Magnesium sheet is to be cut on a squaring shear without being heated. What is the thickest hard-rolled magnesium sheet that should be sheared cold?
FAA-H-8083-31B, ch. 4, p. 4-83
- A0.032 inch
- B0.064 inch
- C0.125 inch
SHOW THE ANSWERHIDE THE ANSWER
THE ANSWER IS B.
0.064 inch
Magnesium needs close shear tolerances and hold-down pressure, and cold shearing has thickness limits: hard-rolled sheet no thicker than 0.064 inch, and annealed sheet no thicker than 1/8 inch. So 0.064 inch is the limit for hard-rolled sheet. 0.125 inch is the limit for annealed sheet, not hard-rolled, and 0.032 inch is well under the limit. Whatever the thickness, the shear is set to a close clearance of no more than 3 to 5 percent of the sheet thickness.
- Q.10
Drop hammer forming cannot hold tolerances as close as a precision method. Why is it still often used for aircraft sheet metal parts?
FAA-H-8083-31B, ch. 4, p. 4-25
- AIt suits parts whose design changes often, or that are needed in short runs
- BIt needs no dies at all, so any shape can be made in a single blow
- CIt leaves the metal harder than any other forming method can
SHOW THE ANSWERHIDE THE ANSWER
THE ANSWER IS A.
It suits parts whose design changes often, or that are needed in short runs
A drop hammer shapes sheet in matched dies by repeated blows, and it cannot work to tolerances as tight as 0.03 to 0.06 inch. It is still often used for sheet metal parts, aircraft components among them, whose design changes often or that are expected to be made only in short runs. It does need dies and many blows, not a single blow, and the handbook claims no special hardness for it.
We wrote these questions for this page from the FAA handbooks. They are not FAA test questions, and none of them comes from our question bank. Each one names the handbook page it was written from, so you can check it.
How a missed code comes back at the oral
Your test report does not show the questions you missed. It prints the ACS code for what each one tested, and a question missed in this subject prints a code that starts AM.II.A. The examiner reads those codes before your oral and practical.
The Airframe oral runs from 4 questions if your written was clean up to 34, because every code you missed adds 1 more. Airframe also carries 11 practical projects, each with 2 questions attached.
Knowledge elements are tested on the written test and the oral; Risk Management elements are tested on the oral and the practical; Skill elements are tested on the practical only. The whole process is on the oral and practical page, and there are cards to practice the spoken half with on FAA A&P oral test practice questions.
Questions people ask about aircraft sheet metal structural repair
Q.01What is bend allowance?
The length of metal the bend itself uses up, measured along the curve of the neutral axis. It depends on the bend radius, the thickness of the metal and the angle of the bend, and it is added to the flat lengths to find how big a piece to cut.
Q.02How close to the edge of a sheet can a rivet go?
Edge distance, measured from the center of the rivet to the edge of the sheet, should be no less than 2 and no more than 4 rivet diameters, and about 2 and a half is recommended. The minimum is 2 diameters for universal head rivets and 2 and a half for countersunk rivets.
Q.03How do you identify a solid rivet?
By the mark on its head, which shows the alloy, and by its part number. In MS20470AD4-6, MS20470 is the universal head, AD is 2117 alloy, the 4 is the diameter in 32nds of an inch and the 6 is the length in 16ths of an inch.
Q.04How is damage to aircraft structure classified?
As negligible damage, damage repairable by patching, damage repairable by insertion, or damage that needs the part replaced. The manufacturer’s structural repair manual gives the limits for each on that aircraft.
Q.05How many aircraft sheet metal structural repair questions are on the FAA A&P Airframe test?
The FAA does not publish a fixed number. Its Companion Guide to the ACS gives the Metallic Structures subject area 5 to 15% of the Airframe test, which is 5 to 15 of the 100 scored questions. That is a range, not a quota, so your own test can land anywhere inside it.
Q.06Which FAA handbook chapter covers aircraft sheet metal structural repair?
Chapter 4 of FAA-H-8083-31B, the Aviation Maintenance Technician Handbook: Airframe, titled "Aircraft Metal Structural Repair". It runs from pages 4-1 to 4-114, and the FAA publishes the whole handbook free as a PDF.
Read the documents, not us
Every fact on this page was read from these on 19 August 2026 and 15 November 2026. They are the authority and we are the summary. If we and one of them disagree, they are right.
- FAA-H-8083-31B, Aviation Maintenance Technician Handbook: Airframe, chapter 4www.faa.gov
- FAA-S-ACS-1, Aviation Mechanic General, Airframe, and Powerplant Airman Certification Standardswww.faa.gov
- FAA-G-ACS-1, Companion Guide to the Aviation Mechanic General, Airframe, and Powerplant Airman Certification Standards: the written test blueprints (pages 13 and 14) and chapters 6 and 7www.faa.gov
- FAA, Frequently Missed Knowledge Test ACS Codes, 2nd Quarter CY25www.faa.gov
FREE PLAN · NO CARD · 25 QUESTIONS TO START
The bank holds 445 aircraft sheet metal structural repair questions.
Start with one free set: 25 questions and 25 fill-in-the-gaps from any of our 44 subjects, which cover every ACS subject area. Each question has 3 answer choices, like the FAA A&P tests, with a written explanation behind every answer and, for every answer written from the FAA handbooks, the chapter it came from. It needs no card. Pro opens the rest of the bank, the full study guides and the timed mock papers.
Start freeOr answer a few first. The free FAA A&P practice test runs on the page, with no account.